Evaluation of multi-layered graphene nano-platelet composite coatings for corrosion control part II – Cathodic delamination kinetics

Delamination Oxygen permeability Galvanic cell
DOI: 10.1016/j.corsci.2018.03.014 Publication Date: 2018-03-18T18:30:37Z
ABSTRACT
Abstract In-situ Scanning Kelvin probe (SKP) measurements are used to follow the corrosion-driven cathodic delamination kinetics of model coatings comprising graphene nano-platelets (GNP) dispersed in polyvinylbutyral (PVB) adherent to iron and zinc (galvanised steel). To reduce delamination rates by >90% (relative to unpigmented PVB) a GNP volume fraction of 0.056 is required on iron but only 0.028 on zinc. On this basis, together with work function and O2 permeability data it is proposed that the GNP acts principally to slow through-coating oxygen transport on iron; whereas on zinc a galvanic couple forms between zinc and GNP, displacing cathodic oxygen reduction.