Structure and magnetic properties of Fe-Co nanoparticles prepared by polyol method
02 engineering and technology
0210 nano-technology
DOI:
10.1016/j.physb.2017.10.039
Publication Date:
2017-11-02T05:32:48Z
AUTHORS (5)
ABSTRACT
Abstract Fe100−xCox (x = 25 − 45) nanoparticles have been successfully prepared from FeCl2 and Co(C2H3O2)2 by thermal decomposition process in solution of polyethylene glycol and NaOH (polyol method). The influence of pH level and Co concentration on structure and magnetic properties of the Fe-Co nanoparticles were investigated. The X-Ray Diffraction (XRD) results confirm the formation of a body centered cubic single phase of the Fe(Co) nanoparticles. The Scanning Electron Microscopy (SEM) images show the grain size of the samples is about 60 nm. Saturation magnetization the Fe-Co nanoparticles strongly depends on the Co concentration and pH level in the fabrication process. The optimal pH level and Co concentration for the Fe-Co nanoparticles were found to be 7 and 35 at%, respectively. A quite high saturation magnetization of 228 emu/g has been achieved for the Fe-Co nanoparticles.
SUPPLEMENTAL MATERIAL
Coming soon ....
REFERENCES (26)
CITATIONS (13)
EXTERNAL LINKS
PlumX Metrics
RECOMMENDATIONS
FAIR ASSESSMENT
Coming soon ....
JUPYTER LAB
Coming soon ....