ABSTRACT
For flexible displays, recovery and relaxation of acrylic pressure-sensitive adhesives (PSA) must be enhanced; however, only a few studies have focused on their optimization. High cross-linking density the PSA leads to improved but deteriorates stress relaxation; thus, it is difficult perform optimization by simply controlling density. Herein, was determined that UV-patterned with both high low densities in single layer enables relaxation. By introducing PSA, elasticity largely deteriorated significantly improved, compared nonpatterned this effect enhanced increases applied strain. Thereby, were well-optimized values above 71% at 300% The had, respectively, positive negative correlation storage modulus.
SUPPLEMENTAL MATERIAL
Coming soon ....
REFERENCES (31)
CITATIONS (36)
EXTERNAL LINKS
PlumX Metrics
RECOMMENDATIONS
FAIR ASSESSMENT
Coming soon ....
JUPYTER LAB
Coming soon ....